MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Konson DPG Rubber Accelerator
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Dephenyl Guanidine (D)

Molecular Formula: C13H13N3

CAS#: 102-06-7

Properties: Relative density is 1.12~1.20g/cm3, soluble in alcohol, acetone and benzene, slightly soluble in carbon tetrachloride. It is stable in open air.

Applications: It acts as middle-speed accelerator, suitable for natural and synthetic rubber, and also can be used as activator for kinds of thiazole, thiuram and sulfenamide. It acts as plasticizer and plastic-divider on chloroprene rubber, especially suitable for rubber products such as tire, rubber shoes, and so on. DPG is regulated for use in articles in contact with food as specified under FDA 21 CFR177.2600 and under BgVV XXI, Categories 3-4.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 - 1.20 g/cc
Molecular Weight 211 g/mol
Ash <= 0.30 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 145 °CInitial
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
AppearanceWhite or grey white powder or granular
Assay>97%
Heat Loss<0.3%
Sieve residue<0.1%150µm
 <0.5%63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS047 / 256092

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.