MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Vinnolit® E 74 CC PVC for Paste Application
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® E 74 CC PVC for paste application. Vinnolit® E 74 CC is a fine-particle, paste making emulsion homopolymer giving plastisols with a medium viscosity and good shelf life. Pastes with a medium plasticizer content are pseudo plastic over the entire shear range. Vinnolit® E 74 CC is a special grade suitable for automotive applications such as foam and top coats in vacuum-thermoformed artificial leather with good emboss retention. Vinnolit® E 74 CC is characterized by: exceptionally low fogging values, good vacuum-formability in deep drawing, excellent emboss retention, good foam ability.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %ISO 1269
Apparent Bulk Density 0.420 g/cc0.0152 lb/in³ISO 60
Particle Size <= 63 µm<= 63 µm<= 3.0% Retained on 0.063 mm Sieve; DIN EN ISO 53195
Viscosity Test 141 cm³/g1.41 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
Emulsifier ContentMedium
Fogging Characteristic (gravimetric)<=0.5 mgDIN EN ISO 75201
K-Value74ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINNO930 / 291127

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.