MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Pinnacle Thermocouple Protection Tubes O'-Sialon (Bonded Silicon Carbide) TCPT
Categories: Ceramic; Carbide

Material Notes: The robust properties of Pinnacle Thermocouple Protection Tubes make it a superior alternative to competitive tubes in temperature measurement, maintenance and product life areas.

Applications

  • Crucible furnaces
  • Degassing crucibles
  • Holding furnaces
  • Casting areas

Advantages

  • Non-wetting to aluminum and its alloys
  • Less dross build up at metal line
  • Superior response time
  • Narrow temperature control band for energy conservation
  • Excellent thermal shock resistance
  • Longer life

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
Open Porosity 18.1 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 0.0780 GPa
Modulus of Rupture 0.0340 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.40 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 8.97 W/m-K
@Temperature 720 °C
 9.05 W/m-K
@Temperature 540 °C
 10.21 W/m-K
@Temperature 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pt-10% Rh Alloy, Annealed
Pyrotek PTB 2200 Structural Board
Overview - Alumina, 98%, Al2O3
Pyrotek PROSILY G-10R Graphite Lubricant/Coating
Pyrotek PROSILY G-11R Graphite Lubricant/Coating

CPYRO208 / 1925

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.