MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay LTM® 202
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: LTM202 is a high temperature tooling matrix system offering improved handling characteristics and, after appropriate post-cure, thermal cycling capability of up to 200°C (392°F). LTM202 is supplied in standard prepreg and DForm Deformable Composite System formats for the manufacture of high temperature composite tooling.

Features & Benefits:

  • Out life at 21°C (70°F): prepreg 4 days and DForm 2 days
  • Storage at -18°C (0°F): prepreg 12 months and DForm 6 months
  • Prepreg and DForm available formats
  • Minimum cure temperature of 45°C (113°F)
  • Autoclave cure
  • Free-standing post-cure
  • Improved handling characteristics
  • 180°C (356°F) service temperature

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³Cured resin
Storage Temperature -18.0 °C-0.400 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.60 µm/m-°C1.44 µin/in-°FDform
 2.70 µm/m-°C1.50 µin/in-°FStandard tooling
Maximum Service Temperature, Air 200 °C392 °F
Glass Transition Temp, Tg 210 °C410 °FDMA E' onset Tg
Shrinkage 0.021 %0.021 %Dform
 0.045 %0.045 %Standard tooling
 
Processing PropertiesMetricEnglishComments
Cure Time  480 min
@Temperature 60.0 °C
8.00 hour
@Temperature 140 °F
 720 min
@Temperature 55.0 °C
12.0 hour
@Temperature 131 °F
 960 min
@Temperature 50.0 °C
16.0 hour
@Temperature 122 °F
 1440 min
@Temperature 45.0 °C
24.0 hour
@Temperature 113 °F
Gel Time  240 min
@Temperature 60.0 °C
240 min
@Temperature 140 °F
 396 min
@Temperature 55.0 °C
396 min
@Temperature 131 °F
 540 min
@Temperature 50.0 °C
540 min
@Temperature 122 °F
 720 min
@Temperature 45.0 °C
720 min
@Temperature 113 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Resole, Glass Fiber Filled
Overview of materials for Phenolic, Carbon Fiber Composite

PCYTED196 / 180498

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.