MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Henkel Electrodag® PF-407C™ Conductive Polymer
Categories: Polymer

Material Notes: Electrodag™ PF-407C™ polymer thick film is designed for production of low voltage circuitry on polyester film and solvent sensitive substrates such as polycarbonate.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³
Solids Content 35 - 39 %35 - 39 %
Filler Content 35 - 39 %35 - 39 %Carbon
Viscosity 35000 - 50000 cP35000 - 50000 cP
Thickness 6.00 - 10.0 microns0.236 - 0.394 mil
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 20 ohm20 ohm
 
Processing PropertiesMetricEnglishComments
Cure Time 0.250 - 0.500 min0.00417 - 0.00833 hour
 
Descriptive Properties
Adhesion5B (excellent)
Conductive Filler TypeCarbon
Material TypeReady-To-Use Formulation
Recommended SubstratesPolyester film, Polyimide film, Polycarbonate, Paper and Cardboard
Solvent SystemMEK, MIBK, acetone or similar solvents

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Electrodag® PD-056 Conductive Resin
Henkel Electrodag® 965 SS Conductive Ink
Henkel Electrodag® 461 SS Conductive Ink
Henkel Electrodag® 440 AS EMC Coating
Henkel Acheson™ PM-500™ Conductive Coating

PFLEXCM18 / 179420

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.