MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Pellethane® 2363-75D TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pellethane 2363-75D is a thermoplastic polyurethane elastomer

Features: USP Class VI

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0080 in/inMD, 1.6mm thick plaques
Linear Mold Shrinkage, Transverse 0.0030 - 0.0070 in/in1.6mm thick plaques
Melt Flow 28 g/10 min
@Load 2.16 kg,
Temperature 224 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76ASTM D2240
Tensile Strength, Ultimate 5810 psiASTM D412
Flexural Modulus 1300 MPaASTM D790
Tear Strength 257 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 55
@Load 1.00 kg
H-22 (coarser); ASTM D1044
 
Thermal PropertiesOriginal ValueComments
CTE, linear 88.7 µm/m-°CASTM D696
Vicat Softening Point 116 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 205 - 220 °CExtrusion
 210 - 225 °CMolding
Mold Temperature 15.0 - 60.0 °CExtrusion
Drying Temperature 100 - 110 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Pellethane® 2363-65D TPU
Lubrizol LifeSciences Tecoflex® EG-72D TPU - Clear
Lubrizol Estane® S375D Thermoplastic Polyurethane
Covestro Desmopan® 9885DU TPU
Lubrizol LifeSciences Tecoflex® EG-68D TPU - Clear

PLUBR9028 / 203595

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.