MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SCIGRIP SG140 A Methacrylate Adhesive + SG115 B Activator
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: SCIGRIP® SG100 Series Methacrylate Adhesives are two-component, 10:1 mix ratio products for bonding thermoplastics, metals, composites and combinations thereof. These bright white, UV resistant products are suited for color critical applications without compromising physical properties.

Features: UV resistant, Minimal surface preparation, Non-sag handling characteristics, Excellent environmental resistance, Excellent fatigue, impact and shock load resistance.

Information provided by SCIGRIP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³Adhesive
 1.00 g/cc0.0361 lb/in³Mix
 1.48 g/cc0.0535 lb/in³Activator
Viscosity 70000 - 180000 cP70000 - 180000 cPActivator
 150000 - 220000 cP150000 - 220000 cPAdhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 15.5 - 17.2 MPa2250 - 2500 psi
Elongation at Break 15 - 35 %15 - 35 %
Tensile Modulus 0.621 - 0.758 GPa90.0 - 110 ksi
Adhesive Bond Strength 13.8 - 16.5 MPa2000 - 2400 psiLap Shear
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 80.0 - 100 min
@Temperature 23.9 °C
1.33 - 1.67 hour
@Temperature 75.0 °F
Fixture Time
Working Life 35.0 - 45.0 min
@Temperature 23.9 °C
35.0 - 45.0 min
@Temperature 75.0 °F
 
Descriptive Properties
ColorOff WhiteAdhesive
 WhiteActivator
 WhiteMix
Mix Ratio10:1 A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCIGR952 / 243176

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.