MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Riteflex® 447 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex 447 is a nominal 47 Shore D thermoplastic polyester polyester elastomer with a high melting point and excellent mechanical properties.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Water Absorption 0.50 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.013 - 0.018 cm/cmISO 294-4
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 240 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPaISO 527-1/2
Elongation at Break 800 %ISO 527-1/2
Tensile Modulus 95.0 MPa50mm/min; ISO 527-2/1A
Flexural Strength 6.00 MPaISO 178
 4.00 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 90.0 MPaISO 178
Resilience 59Bayshore, %
Izod Impact, Notched (ISO) NB
@Temperature -30.0 °C
ISO 180/1U
 NB
@Temperature 23.0 °C
ISO 180/1U
 NB
@Temperature -30.0 °C
ISO 180/1A
Charpy Impact, Notched NBISO 179/1eA
 45.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+12 ohm-cmASTM D257
 4.00e+14 ohm-cmIEC 60093
Surface Resistance 2.00e+15 ohmIEC 60093
Dielectric Constant 4.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 13.0 kV/mmIEC 60243-1
 310 V/milshort term; ASTM D149
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VASTM D3638
 >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 220 µm/m-°CISO 11359-2
Melting Point 212 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °CISO 75-1, -2
Flammability, UL94 HB
 HB
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Riteflex® 640A TPC, Unfilled
Celanese Riteflex® 425 TPC, Unfilled
Celanese Riteflex® 435 TPC, Unfilled
Celanese Riteflex® 265B TPC
Celanese Riteflex® 440 TPC, Unfilled

PHCQ450 / 178905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.