MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.

Key applications for Akulon:

  • Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectors
  • Consumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, Transportation
  • E&E: Low voltage switch gear/power distribution, Lighting, Power connectors
  • Film: Specialty and barrier films

Information provided by DSM.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/cc(DAM); ISO 1183
Water Absorption 6.2 %DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 1.8 %Humidity Absorption (DAM); Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cmDAM; ISO 294-4
 0.0050 cm/cmDAM; ISO 294-4
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+15 ohmIEC 60093
Comparative Tracking Index >= 600 VPLC 0; UL 746A
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10°C/min (DAM); ISO 11357-1/-3
UL RTI, Electrical 65.0 °C
@Thickness 1.50 mm
UL746B
 65.0 °C
@Thickness 0.750 mm
UL746B
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.750 mm
UL746B
 65.0 °C
@Thickness 1.50 mm
UL746B
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 1.50 mm
UL746B
 65.0 °C
@Thickness 0.750 mm
UL746B
 
Descriptive Properties
Flame RetardantYes
Flame Retarding AgentYes
Heat Stabilized or Stable to HeatYes
Injection MoldingYes
Release AgentYes
RSV Formic Acid2.25 g/100mlISO 307
With FillersYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa PA66-T15 15% Mineral Filled PA66
Domo TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY
Envalior Akulon® K224-G3 PA6-GF15, Conditioned, 15% Glass Filled
Envalior Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry)
Envalior Akulon® K222-KMV5 /A PA6-MD25 FR(30)

PDSMEU060 / 31151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.