MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SEKISUI SPI KYDEX® FST CLR Thermoplastic sheet
Categories: Polymer; Thermoplastic

Material Notes: KYDEX® FST CLR is a proprietary, high performance thermoplastic sheet formulated to meet all Airbus and Boeing toxicity requirements for transparent aircraft interior components.

KYDEX® FST CLR meets all flame, smoke, and heat release requirements set forth in Federal Aviation Regulations (FAR) 25.853 paragraphs (a) and (d) as well as toxicity requirements for Airbus (ABD0031)and Boeing (BSS7239). Its excellent fabrication characteristics make it the ideal material to form two and three dimensional aircraft components.

Suggested Application:

  • Privacy screens
  • Class dividers
  • Decorative accents
  • Backlit panels
Features:
  • Meets the stringent requirements of FAR 25.853(a) and (d) in all thicknesses and colors
  • Meets toxicity smoke requirements of Airbus (ABD0031) and Boeing (BSS7239)
  • Excellent fabrication and formability characteristics that allows for tight tolerance control

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Water Absorption 0.110 %
@Time 86400 sec
0.110 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 125125ASTM D785
Tensile Strength, Yield 77.2 MPa11200 psiASTM D638
Elongation at Break 94.0 %94.0 %ASTM D638
Tensile Modulus 2.358 GPa342.0 ksiASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 2.51 GPa364 ksiASTM D790
Compressive Yield Strength 88.3 MPa12800 psiASTM D695
Compressive Modulus 2.53 GPa367 ksiASTM D695
Bearing Yield Strength <= 325 MPa<= 47100 psiASTM D953
 25.6 MPa
@Strain 4.00 %
3710 psi
@Strain 4.00 %
ASTM D953
Poissons Ratio 0.4390.439ASTM D638
Shear Strength 80.0 MPa11600 psiASTM D732
Gardner Impact >= 72.3 J>= 53.3 ft-lbDrop Dart Impact, GE; ASTM D5420
Instrumented Impact Total Energy 76.3 J56.3 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.1 kV/mm409 kV/inoil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 57.5 µm/m-°C31.9 µin/in-°FASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 124 °C255 °Fannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80.0 %
@Thickness 2.00 mm
80.0 %
@Thickness 0.0787 in
ASTM D1003
 
Descriptive Properties
Vertical BurnPass60 and 12 sec; FAR 25.853(a)(i) and FAR 25.853(a)(ii)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS515 / 325255

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.