MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem PROAID® AC-18-DSA Process Aids
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: PROAID AC-18-DSA is a saturated stearyl amine primarily used as a remarkable internal mill release in rubber articles. Proaid AC 18-DSA also acts as a process aid in all polymers. CAS # 124-30-1.

Applications: Proaid AC-18-DSA’s promotes release of all types of rubber from rubber mills and calendars. The same chemistry has been found to be the “mill release of choice” for sticky ethylene/acrylic elastomers, ethylene/vinyl acetate, and epichlorohydrin. 0.5 phr in peroxide cured FKM has proven to be an excellent mill as well as mold release. Even general-purpose elastomers like SBR and polychloroprene that are causing mill sticking will release better. The excellent mill and calendar release will carry over to mold release as well. Every production facility that mills rubber should keep Proaid AC-18-DSA handy for troublesome sticking problems. The low melt point facilitates ease of adding Proaid AC-18-DSA on the mill (get it in early in mill mixes so sticking does not get started). Suggested Loadings: 0.50 - 2.00 phr for greatly reduced mill and calendar sticking. A synergistic effect can be found with a combination of Proaid AC-18-DSA (1.0 phr), calcium or zinc stearate (1.5 phr) and Proaid Plus (1.0 phr) for extreme cases of sticking. Usually AC-18-DSA is sufficient by itself to achieve good mill release. The only caveat with DSA is the cure activation that occurs in sulfur cures (it is an amine after all). Adding a good retarder and possibly reducing some accelerator may need to be done to compensate for this effect.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.790 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 0.50
 
Descriptive Properties
Appearanceflakes/powder
Iodine Value2.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH364 / 315282

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.