CirculenRecover PPC TKC 273N NA C Black is a 20% mineral Reinforced copolymer polypropylene resin for automotive injection molding applications that contains recycled polypropylene resin that features high rigidity and is available in Classic Black color pellet form. Status: Developmental Availability: North America Application: Automotive Parts; Instrument Panels; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Flow; Good Impact Resistance; Good Processability; High Stiffness Information provided by LyondellBasell. |