MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Danquinsa DANCOLOR® MB-CF-90056 Color master batch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCOLOR® MB-CF-90056 is a color master batch based on TPU-, which will be delivered in form of white colored even granules. This color concentrate is mainly used for the coloring of thermoplastic polyurethane (based on polyester or polyether) by the extrusion-, injection molding and calender processing. A very high quality coloration can be reached.

Application: DANCOLOR MB-CF-90056 can be applied and mixed with all products out of our PEARLTHANE®- or PEARLCOAT®- range ( based on polyester or polyether ) which find their application by extrusion, injection molding or calendering. An addition of 2% ( calculated by the weight of the TPU ) is recommended. If there is a requirement by the end product, higher doses can also be considered.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D-1875
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 °C392 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hour
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Color index no.RAL 90056
Composition0.6Carbon pigments
Light fastness8(1-8) blue scale, DIN 53 389

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ076 / 294496

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.