MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nexeo® HIVAL® 500354 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Features:
  • BPA Free
  • Food Contact Acceptable
Uses Pails

Agency Ratings:

  • FDA 21 CFR 177.1520(c) 3.1

    FDA 21 CFR 177.1520(c) 3.2

RoHS Compliance: RoHS Compliant

Forms: Pellets

Processing Method:

  • Blow Molding
  • Extrusion

Information provided by Nexeo® Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.953 g/ccASTM D1505
Environmental Stress Crack Resistance 25 hourF50; ASTM D1693
Melt Flow 0.38 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66ASTM D2240
Tensile Strength, Yield 390 psiASTM D638
Elongation at Break >= 500 %ASTM D638
Flexural Modulus 180000 psiASTM D790
Tensile Impact Strength 120 ft-lb/in²ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 165 °FASTM D648
Vicat Softening Point 262 °FASTM D1525
Brittleness Temperature >= -76.0 °FF50; ASTM D746
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 330 - 360 °FBlow Molding
Zone 1 380 - 440 °FExtrusion
Zone 3 390 - 450 °FExtrusion
Zone 5 400 - 470 °FExtrusion
Die Temperature 140 - 450 °FExtrusion
Head Temperature 375 °FBlow Molding
Mold Temperature 60.0 °FBlow Molding
Drying Temperature 170 - 175 °FExtrusion
Dry Time 2.00 hourExtrusion
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane
Sterigenics Raprex® R100D Branched High Density Polyethylene
Kazanorgsintez PE80B-285SL High Density Polyethylene Composite, Film Grade
Entec Hypel® PEHD30/.950 HDPE

PNEXEO913 / 197597

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.