MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Adell WL-38 40% Glass and Mineral Reinforced PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass/Mineral Reinforced

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D792
Water Absorption 0.050 %0.050 %24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8787ASTM D785
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Ultimate 124 MPa18000 psiASTM D638
Flexural Strength 175 MPa25400 psiASTM D790
Flexural Modulus 8.35 GPa1210 ksiASTM D790
Compressive Yield Strength 145 MPa21000 psiASTM D695
Izod Impact, Notched 0.694 J/cm
@Thickness 3.17 mm
1.30 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 232 - 249 °C450 - 480 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 243 °C470 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET
A. Schulman POLYBATCH™ White 8153/UV2 Concentrate Based In Polyethylene
3M AC-770 Class B-1 Aerospace Sealant

PDELL81 / 98139

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.