System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Imerys Minspar™ 200 Feldspar
Categories:
Ceramic
;
Clay
;
Feldspar Clay
;
Oxide
;
Silicon Oxide
Material Notes:
Minspar 200 is 200 mesh flotation grade soda Feldspar used in the ceramic whiteware industry for sanitaryware, dinnerware, floor and wall tile, artware and glazes.
Information provided by Imerys
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
44.0
lb/ft³
loose
70.0
lb/ft³
packed
Brightness
94 %
Dry Brightness (Green Filter)
Particle Size
5.0
µm
19% finer than
10
µm
40% finer than
12
µm
mean
20
µm
72% finer than
30
µm
87% finer than
Particle Mesh Size
20
Mesh
0% retained
30
Mesh
0% retained
40
Mesh
0% retained
100
Mesh
trace retained
140
Mesh
trace retained
170
Mesh
0.1% retained
200
Mesh
0.3% retained
325
Mesh
3.6% retained
pH
8.7
Specific Surface Area
0.90
-
1.2
m²/g
Mechanical Properties
Original Value
Comments
Hardness, Mohs
6.0 - 6.5
Optical Properties
Original Value
Comments
Refractive Index
1.53
Component Elements Properties
Original Value
Comments
Al2O3
18.5 %
CaO
1.5 %
Fe2O3
0.060 %
H2O, Water
0.10 %
K2O
4.1 %
Loss on Ignition(%)
0.30 %
Na2O
6.5 %
SiO2
68.6 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Imerys Minspar™ 10 Ground Feldspar
Imerys Minspar™ 7 Ground Feldspar
Imerys Minspar™ 4 Ground Feldspar
Old Hickory FC-340 Tennessee Ball Clay
Old Hickory S-4 Tennessee Ball Clay
CIMERY011 / 88361
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.