MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Gear Compounds EP J, ISO 320
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Gear Compounds EP J are multipurpose gear lubricants.

They are formulated with highly refined, high viscosity index paraffinic base oils and a new generation sulfurphosphorus additive system. Chevron Gear Compounds EP J contain extreme pressure, antiwear and emulsibility additives; oxidation, rust, corrosion and foam inhibitors; a pour point depressant; and a metal deactivator to protect copper or copper alloys from corrosion.

They are specifically designed to meet or exceed the performance requirements of Joy Technologies specifications for transmission oils.

Chevron Gear Compounds EP J are formulated to give high film strength and load-carrying capacity. Gear teeth are protected from wear, all types of surface distress, and premature failure.

They provide improved thermal and oxidation stability to prevent degradation under severe operating conditions and provide longer lubricant life. They are designed to form a stable emulsion with contaminating water.

Applications

Chevron Gear Compounds EP J are recommended for use in Joy Technologies transmissions or other similar applications where water emulsifying gear oils are required.

Chevron Gear Compounds EP J meet Joy specifications TO-MEP (ISO 220), TO HEP (ISO 320) and TO HD (ISO 460).

For customers that do not have water emulsibility as a requirement, Chevron Gear Compounds EP or Chevron Ultra Gear Lubricants are recommended. Chevron Ultra Gear Lubricants can be used in industrial applications where overloading, severe operating conditions, high lubricant operating temperatures, or other problems are encountered.

Key Words: CPS Number: 226808; MSDS Number: 7477
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 26 °
Viscosity Measurement 113Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1689 SUS
Saybolt Viscosity at 210°F 134 SUS
Kinematic Viscosity at 40°C (104°F) 320 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 27.2 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Falex Load Test >= 3750 lbASTM D3233
 
Thermal PropertiesOriginal ValueComments
Pour Point -18.0 °CASTM D97
Flash Point 244 °CASTM D92
 
Descriptive Properties
Corrosion, Copper Strip Test 3h0 at 100°C
Emulsibility ASTM D1401, mL H20 at 48 h0
Foaming Stability, mL0
Foaming Tendency, mL0
FZG Gear Wear Test, Failure Load Stage12
Oxidation, ASTM D2893, % Viscosity Increase3.6
Rust Prevention, ASTM D665Pass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV205 / 74820

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.