MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ductile Iron compression grade 80-55-06
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Carbon represents the total carbon in the listed composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. For example, 80-55-06 ductile iron is specified to have a minimum tensile strength of 80 ksi (552 MPa), a yield strength of 55 ksi (379 MPa) and an elongation of 6%. Determined for a single temperature of ductile iron, heat treated to approximate various standard grades. Properties were obtained using test bars machined from 25 mm keel blocks.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.10 - 7.20 g/ccTypical value of ductile iron
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 192
Hardness, Knoop 213Converted from Brinell
Hardness, Vickers 201Approximated. Converted from Brinell hardness.
Tensile Strength, Yield 386 MPa
@Strain 0.2 %
Modulus of Elasticity 165 GPa
Poissons Ratio 0.31
Shear Modulus 63.0 GPacalculated
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 3.6 - 3.8 %
Cerium, Ce 0.0050 - 0.20 %
Chromium, Cr 0.030 - 0.070 %
Copper, Cu 0.15 - 1.0 %
Iron, Fe 90.738 - 94.175 %
Magnesium, Mg 0.030 - 0.060 %
Manganese, Mn 0.15 - 1.0 %
Molybdenum, Mo 0.010 - 0.10 %
Nickel, Ni 0.050 - 0.20 %
Phosphorus, P <= 0.030 %
Silicon, Si 1.8 - 2.8 %
Sulfur, S <= 0.0020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ductile Iron grade 80-55-06
Ductile Iron tension grade 80-55-06
Ductile Iron torsion grade 80-55-06
Ductile Iron tension grade 60-40-18
Ductile Iron tension grade 65-45-12

MDFE21 / 12018

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.