MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zylog Neoplast® 180 C Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Neoplast 180 C is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.

RoHS Compliant, UV Stabilized

Information provided by Zylog Plastalloys Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ASTM D 2240
 86
@Treatment Temp. 150 °C,
Time 605000 sec
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 95.0 kg(f)/cm²500 mm/min; ASTM D 412
 105 kg(f)/cm²
@Treatment Temp. 150 °C,
Time 605000 sec
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 550 %500 mm/min; ASTM D 412
 495 %
@Treatment Temp. 150 °C,
Time 605000 sec
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.925 ksi
@Strain 100 %
500 mm/min; ASTM D 412
Tear Strength 50.0 kg(f)/cm500 mm/min; ASTM D 624
Compression Set 48 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM B 395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °CContinuous; SAE J 2236
Brittleness Temperature -60.0 °CASTM D 746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zylog Neoplast® 180 FT EB Thermoplastic Vulcanizate
Zylog Neoplast® 180 HOFR Thermoplastic Vulcanizate
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer
A. Schulman Diamond Softflex® SF 7001 Thermoplastic Vulcanizate (TPV)
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer

PZYLOG957 / 157273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.