MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
INEOS Styrolution K-Resin® DK11E SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Product Description: K-Resin® DK11E makes a clear, stiff, very tough, high gloss film suitable for applications such as candy twist wrap, shrink sleeves and overwrap. K-Resin® K-Resin® SBC grade designed for blown film extrusion is DK11E.
Features: Excellent Clarity; High Surface Gloss; Good Heat Sealability
Applications: Medical Packaging; Produce Packaging; Twist Wrap; Lidstock and Labeling Film

Availability: Latin America; North America

Features: Block Copolymer; Good Stiffness; Good Toughness; Heat Sealable; High Clarity; High Gloss

Uses: Film; Food Packaging; Labels; Medical Packaging; Packaging

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Blown Film; Extrusion; Film Extrusion

Information provided by INEOS Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccASTM D792
Water Vapor Transmission 5.50 g/100 in²/day0% to 85% RH gradient; ASTM F1249
Oxygen Transmission Rate 420 cc/100 in²/day0% RH; ASTM D3985
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 5000 psiASTM D882
Film Tensile Strength at Yield, TD 3100 psiASTM D882
Film Elongation at Break, MD 110 %ASTM D882
Film Elongation at Break, TD 200 %ASTM D882
1% Secant Modulus 140000 psiTD; ASTM D882
 205000 psiMD; ASTM D882
Dart Drop, Total Energy 0.667 ft-lbPeak Force; ASTM D3763
Elmendorf Tear Strength MD 9.1 gASTM D1922
Elmendorf Tear Strength TD 1.5 gASTM D1922
Dart Drop Test 590 g
@Thickness 660 mm
ASTM D1709
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 185 °FRate B (120°C/h), Loading 1 (10 N); ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze <= 0.90 %ASTM D1003
Gloss 140 %mold temperature 100°F; ASTM D2457
Transmission, Visible 92 %
@Thickness 14000 mm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTYS758 / 311451

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.