MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Vinnolit® P 4472 PVC for Paste Application
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® P 4472 PVC for paste application. Vinnolit® P 4472 is a fine-particle emulsion homopolymer for making PVC pastes. Plastisols based on Vinnolit® P 4472 are distinguished by a low initial viscosity and almost Newtonian flow properties. Principal applications are pastes for compact vinyl wallcoverings, flooring and leather cloth, as well as for coating of woven and non-woven fabrics and of glass strands. The following properties make Vinnolit® P 4472 particularly suited to the manufacture of low-plasticizer and/or highly filled pastes: very low initial viscosity, almost linear flow properties, excellent release effect during contact fusion, high suitability for mechanically blown foam containing silicone based foaming aids.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.30 %<= 0.30 %ISO 1269
Apparent Bulk Density 0.320 g/cc0.0116 lb/in³ISO 60
Particle Size <= 63 µm<= 63 µm<= 1.5% Retained on 0.063 mm Sieve; DIN EN ISO 53195
Viscosity Test 132 cm³/g1.32 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
Emulsifier ContentMedium
K-Value72ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINNO933 / 291130

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.