MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow BETAMATE™ 7200 Polyurethane Prepolymer  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: BETAMATE™ 7200 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It also shows excellent sealer combining medium strength bonding and sealing properties in a wet one-step operation. It can be abraded and is over-paintable with most of the paint systems.

Information provided by Dow

BETAMATE™ is now a DuPont product line, but this specific product was discontinued while BETAMATE™ was a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 - 1.25 g/cc
Viscosity <= 260000 cP(Haake RU 20, 115 OSC, PK 2-1, 0; D= 1s-1)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40 - 50DIN 53 505
Tensile Strength, Ultimate 2.30 - 2.90 MPaDIN 54 504
Elongation at Break 450 %DIN 54 504
Adhesive Bond Strength 1.50 - 2.10 MPaLap Shear Strength (bond thickness: 2mm); EN 1465
Tear Strength 7.00 - 9.00 kN/mASTM D624 Form B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °Ccontinuous (Cured condition)
 120 °Cshort term (Cured condition)
Minimum Service Temperature, Air -40.0 °Ccontinuous (Cured condition)
Shrinkage 5.0 - 6.0 %DIN 52 451
 
Processing PropertiesOriginal ValueComments
Cure Time 1440 min
@Temperature 23.0 °C
50% RH

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow BETAFOAM™ 87100 MDI & PMDI Isocyanate
DuPont BETAMATE™ 73345G Epoxy
DuPont Mobility and Materials Betamate™ 1496V Epoxy Adhesive, Body Shop Grade
Dow BETAFOAM™ 87120 Polyether / Polyol Blend
Dow BETAFOAM™ 89120 Water/Amine catalyst

PZDOW1005 / 30209

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.