MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Armacell OleTex® BDJN 400 Buns, Polyethylene/EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Polyethylene (PE)

Material Notes:

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0641 g/cc0.00231 lb/in³ASTM D3575W
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.621 MPa90.0 psiASTM D3575T
Elongation at Break 340 %340 %ASTM D3575T
Compressive Strength  0.0689 MPa
@Strain 10 %
10.0 psi
@Strain 10 %
ASTM D3575D
 0.0896 MPa
@Strain 25 %
13.0 psi
@Strain 25 %
ASTM D3575D
 0.117 MPa
@Strain 40 %
17.0 psi
@Strain 40 %
ASTM D3575D
 0.152 MPa
@Strain 50 %
22.0 psi
@Strain 50 %
ASTM D3575D
Tear Strength 3.68 kN/m21.0 pliASTM D3575G
Compression Set 16 %16 %ASTM D3575B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 98.9 °C210 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Descriptive Properties
FlammabilityFMVSS302Pass
Thermal Stability<2%24 hrs @ 158°F, ASTM D3575S

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 1241 EVA polymer for compounds, flexible packaging and foam
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding
Arkema Orevac® 18216 Maleic Anhydride modified EVA
Arkema Orevac® 9305 Film EVA-MAH Terpolymer
Arkema Orevac® 9304 Film EVA-MAH Terpolymer

PARMD117 / 186728

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.