MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toray G-85FR Prepreg Laminate with ARAMID Fiber 1000 DENIER 2X2 TWILL AT 186 g/m2 FAW AND 43% RC
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: G-85FR is a resin system developed specifically to meet the needs of the automotive industry. A 10 minute cure time at 325°F makes it suitable for high throughput processes, and its flame retardancy and high heat tolerance make it ideal for racing applications. This system also offers easy handleability, and the capability to achieve a class “A” surface finish.

Information provided by Toray Composite Materials America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 511 MPa74100 psi90° (F2t); ASTM D3039
Tensile Modulus 24.3 GPa3520 ksi90° (E2t); ASTM D3039
Flexural Strength 438 MPa63500 psiASTM D790
Flexural Modulus 21.0 GPa3050 ksiASTM D790
Compressive Strength 115 MPa16700 psiAfter Impact (1500 in-lb/in); ASTM D7137
 188 MPa27300 psi90° (F2C); ASTM D695
Poissons Ratio 0.0690.069
Shear Modulus 1.59 GPa231 ksiASTM D5379
Shear Strength 41.9 MPa6080 psiInterlaminar; ASTM D2344
 59.4 MPa8620 psiASTM D5379
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Temperature 163 °C
0.167 hour
@Temperature 325 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY8049 / 265447

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.