Temper: As Sand Cast Fabrication Properties: Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Soldering, Brazing, Coated Metal Arc Welding, Capacity for Being Cold Worked Applicable Specifications: As Continuous Cast – ASTM B505/B505M; Die Forging – ASTM B283/B283M; Ingot – ASTM B30; Rod, Bar & Shapes – Forgings ASTM B124/B124M |