MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8281 HS GP PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering properties including strength, stiffness, and toughness combined with excellent abrasion resistance and self lubricating characteristics. In addition, the heat stabilizer system extends its retention of properties at elevated temperatures. Chemical resistance is excellent to greases, oils and hydrocarbons. All data is from injection molded specimens with the exception of Drop Weight Impact.

Applications: Ultramid 8281 HS GP is generally recommended for applications such as fuel tanks, chemical storage tanks, hydraulic oil reservoirs, cyclones, and heat resistance containers.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccASTM D792
Moisture Absorption at Equilibrium 1.3 %24 Hours; ASTM D570
 2.7 %50% RH; ASTM D570
 9.5 %Saturation; ASTM D570
Linear Mold Shrinkage 0.0508 cm/cm1/8" bar
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116ASTM D785
Tensile Strength, Yield 20.0 MPa
@Temperature 65.0 °C
ASTM D638
 72.0 MPa
@Temperature 23.0 °C
ASTM D638
 114 MPa
@Temperature -40.0 °C
ASTM D638
Elongation at Break >= 100 %ASTM D638
Flexural Strength 15.0 MPa
@Temperature 121 °C
ASTM D790
 20.0 MPa
@Temperature 90.0 °C
ASTM D790
 30.0 MPa
@Temperature 65.0 °C
ASTM D790
 100 MPa
@Temperature 23.0 °C
ASTM D790
 154 MPa
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 300 MPa
@Temperature 121 °C
ASTM D790
 360 MPa
@Temperature 90.0 °C
ASTM D790
 530 MPa
@Temperature 65.0 °C
ASTM D790
 2690 MPa
@Temperature 23.0 °C
ASTM D790
 2760 MPa
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched (ISO) 45.0 kJ/m²
@Temperature -40.0 °C
ASTM D256
 55.0 kJ/m²
@Temperature 23.0 °C
ASTM D256
Dart Drop, Total Energy 67.8 JBASF
 
Thermal PropertiesOriginal ValueComments
CTE, linear 74.0 µm/m-°CASTM E831
Melting Point 220 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Dry Time 2 - 4 hour
Moisture Content <= 0.20 %
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8350 HS PA6 (Conditioned)
BASF Ultramid® 8270 HS PA6 (Dry)
BASF Ultramid® 8260 HS PA6 (Dry)
BASF Ultramid® 8260 HS PA6 (Conditioned)
BASF Ultramid® B27 03 PA6

PBASG0463 / 132096

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.