Homopolymer, non-oxidized polyethylene wax. STRUKTOL® PE(H)-100 is a versatile polyethylene wax (homopolymer) used in natural and synthetic elastomers. It is used to improve flow and processability. STRUKTOL® PE(H)-100 also provides good release from equipment with improved pigment dispersion and finish to molded articles. FDA Status: 175.105; 175.125; 175.300; 176.180; 176.200; 176.210; 177.1200; 177.1210; 177.2600; 178.3570; 178.3850 |