MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SACO AEI EXTINITY® 0201-125 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: EXTINITY® 0201-125 is a highly filled flame retardant concentrate that is designed to meet a variety of film flame retardant specifications including; MVSS-302, NFPA-701 Small Scale Test and UL-94 VTM-0 flame standards. EXTINITY® 0201-125 can be used in a variety of polyolefin base resin systems including LDPE, LLDPE, HDPE and mixtures of PE. EXTINITY® 0201-125 contains a flame-retardant package that is very thermally stable, UV stable and does not bloom. The brominated fire retardant in 0201-125 is RoHS compliant.

Recommended Applications:
Extrusion: Film, Sheet, Tubing, Jacketing, Cast
Molding: Injection, Thermoforming, Rotational

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.67 g/ccASTM D792
Melt Flow 1.0 - 4.0 g/10 minASTM D1238 Condition E
Storage Temperature 40.0 - 80.0 °F
 
Descriptive Properties
FormYellow Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO026 / 249393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.