MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Sweetbay Magnolia Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Mechanical properties reported according to ASTM D143 at 12 wt% moisture content.

Key Words: Magnolia virginiana, timber, lumber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.450 g/ccOven-dry to green volume ratio
Density 0.465 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 11.5 GPa
Modulus of Rupture 0.0704 GPa
Compressive Strength 3.90 MPaperpendicular
 39.8 MPaparallel
Shear Strength 11.8 MPaparallel
Work to Maximum Load 0.05171 J/cm³
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.140 W/m-K
Shrinkage 4.7 %radial; from green to oven-dry condition based on initial condition when green
 8.3 %tangent
 12.9 %volume
 
Descriptive Properties
CategoryHardwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silver Birch (Gray Birch) Wood
Southern Bluegum Wood
Southern Pine Wood
Southern Red Oak Wood
Swamp Chestnut White Oak Wood

PTSU078 / 100540

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.