MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Free Form™ AIR Fire Safe Lightweight epoxy putty
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: Free Form™ AIR Fire Safe is a lightweight epoxy putty that certifies to the highest flame rating available (E84, Class A). This is a low odor, low shrinkage putty that is unique, inexpensive and easy to use. Free Form™ AIR Fire Safe is mixed by hand with a 1A:1B by volume mix ratio. It offers a long working time and cures overnight at room temperature to a rigid epoxy that is very strong. It can be sanded, shaped and drilled. It will readily accept any paint. Free Form™ AIR Fire Safe can also be color pigmented with UVO™ or Ignite™ colorants. Press Into a Mold - After mixing, Free Form™ AIR Fire Safe can be pressed into a mold to make a lightweight, detailed casting. Apply to Vertical Surfaces - Free Form™ AIR Fire Safe will hold vertical surfaces and can be applied to almost any surface including polystyrene foam for rough sculpting. Free Form™ AIR Fire Safe is suitable for interior/exterior theming applications and general sculpting and is used to make hyper-realistic trees, vines, rocks, and other display elements. Pot Life/Working Time; this material is mass sensitive. The more material you mix at one time, the less time you have to work with it. Working tip; If mixing a large quantity, flatten putty with a rolling pin to reduce mass concentration and extend pot life.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.800 g/cc0.800 g/ccASTM D-1475
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373ASTM D2240
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °FHeat Deflection Temperature; ASTM D-648
 
Descriptive Properties
ColorGrey
Mix Ratio1A:1Bby volume
Mixed ViscosityDough
Specific Volume34.6[in3/lb], ASTM D1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN296 / 296997

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.