MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal KLINGER® top-chem-2003 PTFE Gasketing
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Ideal for low bolt applications or w here flanges are delicate
  • Excellent chemical resistance to acidic and alkaline attack
  • Highly compressible
  • FDA compatible
  • Ideal for higher temperatures and pressures
  • Holds shape for thermal cycles
Permits/Certifications: KTW proposal; DIN-DVGW permit; FDA conformity; TA-Luft certification and Germanischer Lloyd

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³
Thickness 2000 microns78.7 milThickness tested
 
Descriptive Properties
Compressibility18 percentASTM F36
Klinger Cold/Hot Compression38 percent480°F/3,625 psi
 9 percent75°F/3,625 psi
Recovery40 percentASTM F36
Sealability0.01 mg/s mDIN 28090-2
 0.1 ml/minDIN 3535/6
Stress Relaxation13 MPaDIN 52913, 16h 4,350 psi, 300°F
Weight Increase1%H2SO4, 100%: 18h/75°F
 2%NaOH, 33%: 72h/230°F
 5%HNO3, 100%: 18h/75°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTHERM902 / 146055

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.