MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Polynt POLYCOR® 998 Series Enamels
Categories: Polymer; Thermoset

Material Notes: Polynt Composites' POLYCOR® 998 Series Enamels are formulated to be used as topcoats on fiberglass laminates. Enamels are very similar to gel coats except they cure tack-free on the open surface. Enamels are used to seal and hide a substrate. Normally they are used as interior finishes and yield a pigmented surface. POLYCOR® 998 Series Enamels were primarily developed for marine applications; however, they can be used in any FRP application where high performance characteristics are desired. POLYCOR® 998 Series Enamels produce a hard, tough, durable coating that reduces maintenance on composites parts. POLYCOR® 998 Series Enamels cure to a flat finish. Standard enamels should not be used for water immersion service due to potential water spotting and water blistering. Contact a sales representative for a recommendation if water immersion is required. POLYCOR® 998 Series Enamels meet the EPA National Emission Standards for Hazardous Air Pollutants (NESHAP) for both Marine Manufacturing and Reinforced Composites Production. POLYCOR® 998 Series Enamels contain wax. The wax is essential to yielding a tack-free surface in the top coating application. The wax also helps to suppress the volatile organic compounds emitted in to the air. Together the low VOC or HAP content and wax results in:
  • Reduced monomer emissions
  • Less odor
  • Smoother sprayed film (less orange peel)
  • Less overspray
Due to the wax, POLYCOR® 998 Series enamels should not be used as an in-mold coating where they will be backed by laminate or other materials. Delamination could occur. Enamels require only the addition of the proper amount of the appropriate methyl ethyl ketone peroxide to cure. These enamels are available in white or any of the colors listed in the standard gel coat color card. Special colors are available upon request.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 3400 cPRVF #4 Spindle @ 20 rpm
 15000 cPRVF #4 Spindle @ 4 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 82.0 - 88.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 90.0 minTack Free/Dull Gloss Time
Gel Time 10.0 - 18.0 minMethod POLYNT-22-TAS-TM-515.2, 100 g mass, 1.8% Arkema Luperox® DDM-9
 
Descriptive Properties
Sag ResistanceGood @ 20 mils
Thixotropic Index4.5-72/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9230 / 231825

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.