MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLOY™ FR Resin CX7240U Polycarbonate + ABS (PC+ABS) (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CX7240U Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, medium flow, non chlorinated/brominated UV stabilized flame retardant grade. It has a UL94 V0@.75mm, 5VA@3.0mm and 5VB@1.5mm flame rating. This grade has improved chemical resistance compared to standard PC/ABS blends and is a good candidate for thin wall applications.

Features: Hydrolytic Stability,Chemical Resistance,Flame Retardant,UV Resistant,Non-Chlorinated,Non-Brominated,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.0400 %0.0400 %Injection Molding
 0.100 %0.100 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %0.20 %ISO 62-1
Viscosity 15 cP
@Load 2.16 kg,
Temperature 260 °C
15 cP
@Load 4.76 lb,
Temperature 500 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 260 °C
16 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527
 58.0 MPa8410 psi50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ASTM D638
 65.0 MPa9430 psi50 mm/min; ISO 527
Elongation at Break 90 %90 %50 mm/min; ISO 527
 100 %100 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527
 4.1 %4.1 %50 mm/min; ASTM D638
Tensile Modulus 2.53 GPa367 ksi1 mm/min; ISO 527
 2.95 GPa428 ksi50 mm/min; ASTM D638
Flexural Strength 96.0 MPa13900 psiyield, 2 mm/min; ISO 178
 104 MPa15100 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
 2.75 GPa399 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 500 J369 ft-lbASTM D256
 100 J
@Temperature -30.0 °C
73.8 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 65.0 J47.9 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 0.750 mm
15 - 30 sec
@Thickness 0.0295 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  53.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
29.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 54.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  62.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
34.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 62.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
34.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Hot Ball Pressure Test 75.0 °C167 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
@Thickness 3.20 mm
212 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C199 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 89.0 °C
@Thickness 3.20 mm
192 °F
@Thickness 0.126 in
unannealed; ASTM D648
 99.0 °C
@Thickness 6.40 mm
210 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 106 °C223 °FRate B/50; ASTM D1525
 110 °C230 °FRate B/50; ISO 306
 113 °C235 °FRate B/120; ISO 306
UL RTI, Electrical 90.0 °C194 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746B
Flammability, UL94  V-2
@Thickness >=0.400 mm
V-2
@Thickness >=0.0157 in
UL 94
 V-1
@Thickness >=0.600 mm
V-1
@Thickness >=0.0236 in
UL 94
 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
UL 94
 5VB
@Thickness >=1.50 mm
5VB
@Thickness >=0.0591 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
Glow Wire Ignition Temperature  800 °C
@Thickness 0.750 mm
1470 °F
@Thickness 0.0295 in
IEC 60695-2-13
 800 °C
@Thickness 1.50 mm
1470 °F
@Thickness 0.0591 in
IEC 60695-2-13
 800 °C
@Thickness 2.00 mm
1470 °F
@Thickness 0.0787 in
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 265 - 300 °C509 - 572 °F
Zone 2 260 - 300 °C500 - 572 °F
Zone 3 265 - 300 °C509 - 572 °F
Melt Temperature 270 - 300 °C518 - 572 °FInjection Molding
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 90.0 °C194 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00380 - 0.00760 cm0.00150 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80034 / 287981

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.