Base Polymer: Thermoplastic Vulcanisate PP/EPDM-Elastomer Special Features: Good weathering resistance, resistant to alkalis, resistant to ozone, resistant to hot air, hydrolysis resistant, high flow, inherent color Market Segment: Electrical and Electronic, household goods, Sport and Leisure Application Area: Injection molded parts, Food Contact Applications Typical Applications: Seals, handles, racking/shelving, impact protection/shock absorber, protection cap Information provided by Albis Plastics |