MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene LP510034 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petrothene LP510034 is selected by customers for use in large-part blow molding of durable goods and for deep-draw sheet extrusion / thermoforming applications. LP510034 exhibits excellent impact resistance and excellent environmental stress crack resistance.

Availability: North America

Application: Industrial Packaging; Jerry Cans; Structural Parts

Market: Rigid Packaging

Processing Method: Extrusion Blow Molding; Sheet and Profile Extrusion

Attribute: High ESCR (Environmental Stress Cracking Resistance)

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D1505
ESCR 100% Igepal® >= 1000 hourCond B; ASTM D1693
Melt Flow 11.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65.0ASTM D2240
Tensile Strength, Yield 25.5 MPaASTM D638
Elongation at Break >= 800 %ASTM D638
Flexural Modulus 1140 MPa1% Secant; ASTM D790
Tensile Impact Strength >= 420 kJ/m²ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CUnannealed; ASTM D648
Vicat Softening Point 122 °CASTM D1525
Brittleness Temperature <= -76.0 °CF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9723 / 324658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.