MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Mobility and Materials Multiflex™ TES G90 A 520 Styrenic Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Thermoplastic Elastomer based Styrenic

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Spiral Flow 51.0 cm20.1 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 8.50 MPa1230 psiISO 527-1/-2 or ISO 37
Tensile Stress at Strain 8.60 MPa
@Strain 100 %
1250 psi
@Strain 100 %
ISO 527-1/-2 or ISO 37
Elongation at Break 160 %160 %ISO 527-1/-2 or ISO 37
Tear Strength 48.0 kN/m274 pliparallel; ISO 34-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 215 °C419 °FOptimum, Injection
Mold Temperature 35.0 °C95.0 °FOptimum, Injection
 25.0 - 45.0 °C77.0 - 113 °FInjection
Drying Temperature 65.0 °C149 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 
Descriptive Properties
ColorBlack
CompatibilityPolyolefins
Drying RecommendedyesInjection
Injection speedHigh
PolymerTPS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF9332 / 254377

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.