MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexTow® PV42/850 Carbon Fiber - Epoxy Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Physical property data for typical epoxy composite reinced with PV42/850.

HexTow™ PV42/850 (HS-CP-3300) carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. This fiber has been designed for applications that require high composite tensile strength. The fiber can be sized to improve its handling characteristics. HexTow™ PV42/850 (HS-CP-3300) fiber is suggested for use in filament winding for pressure vessels and other similar applications.
The unique properties of HexTow™ PV42/850 (HS-CP-3300) fiber allow structural designers to achieve higher safety margins for strength critical applications.

Information provided by Hexcel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 62 %62 %PV42/850 Fiber Volume %
Filament Diameter 5.1 µm5.1 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 3378 MPa489900 psi
Tensile Modulus 178 GPa25800 ksi
Flexural Modulus 148 GPa21500 ksi
Shear Strength 93.0 MPa13500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXC681 / 322761

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.