MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Free-Cutting Brass, UNS C36000, H04 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Butt Weld, Capacity for Being Hot Formed, Capacity for Being Cold Worked

Common Fabrication Processes: Machining; Roll Threading and Knurling

Typical uses: Terrazzo Strip; Fluid Connectors; Sensor Bodies; Thermostat Parts; Threaded Inserts for Plastic; Fittings; Hardware; Lock Bodies; Hot Combs (to Straighten Hair); Bolts; Screws; Adapters; Automatic Screw Machine Parts; Faucet Components; Fluid Connectors; Gauges; Gears; Nozzles; Pinions; Pneumatic Fittings; Screw Machine Products; Unions; Valve Seats; Valve Stems; Valve Trim; Faucet Seats; Plumbers' Brass Goods; Faucet Stems; Plumbing Fittings

Applicable Specifications: Bar – SAE J461, AMS 4610; SAE J463, ASTM B16/B16M; Rod – SAE J463, AMS 4610, SAE J461, ASTM B16/B16M; Shapes – SAE J461, SAE J463, ASTM B16/B16M; Valves – MILITARY MIL-V-18436; Wire – ASTM B16/B16M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.307 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 78
@Thickness 9.52 mm
 80
@Thickness 6.35 mm
Tensile Strength >= 65.0 ksi
@Thickness 15.9 mm
for Standard
 >= 70.0 ksi
@Thickness 9.52 mm
for Standard
 >= 80.0 ksi
@Thickness 6.35 mm
for Standard
Elongation at Break >= 4.0 %
@Thickness 9.52 mm
for Standard
 >= 6.0 %
@Thickness 15.9 mm
for Standard
Tensile Modulus 14000 ksi
Modulus of Rigidity 5300 ksi
Poissons Ratio 0.32Calculated
Machinability 100 %
Shear Strength 34.0 ksi
@Thickness 9.52 mm
 38.0 ksi
@Thickness 6.35 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm26% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.4 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 67.0 BTU-in/hr-ft²-°F
Melting Point 1630 - 1650 °F
Solidus 1630 °F
Liquidus 1650 °F
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1300 - 1450 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 60 - 63 %
Iron, Fe <= 0.35 %
Lead, Pb 2.5 - 3.0 %
Zinc, Zn 34 - 37.5 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC36000x5 / 292947

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.