MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Addovate® TX PU Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Emulsifier/Stabilizer for the production of polyurethane polyester flexible slabstock foam.

Product information: Before processing Addovate TX has to be thoroughly homogenized by rolling or tumbling the drums or stirring the contents. Addovate TX is usually used in combination with Addovate EM in the manufacture of polyester slabstock foam. With a combination of Addovate TX / Addovate EM, good foaming control resulting in fine cell structure can be achieved. The proportions which should be used are 1.0-3.0 p.b.w. Addovate TX to 100.0 p.b.w. polyester polyol. The following sequence for adding the individual components has proven effective in the manufacture of catalyst compounds: water, catalyst, Addovate EM, Addovate TX. A clear, homogeneous mixture is produced.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³
Water Absorption <= 1.0 %<= 1.0 %
Viscosity 250 - 450 cP250 - 450 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value 6.0 - 8.06.0 - 8.0[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Boiling Point >= 100 °C>= 212 °FInitial
Pour Point -20.6 °C-5.00 °F
Flash Point >= 100 °C>= 212 °FASTM D93, DIN EN 22719
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Appearancebrown liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8232 / 208625

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.