MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ THERMOTUF™ Compound DF004PSI Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOTUF DF004PSI compound is based on Polycarbonate (PC) resin containing 20% glass fiber. Added features of this grade include: Impact Modified, High Flow Ductile, Good Chemical Resistance.

Features: Impact Modified,High Stiffness,Chemical Resistance,High Impact Resistance,High Flow,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 10 cP
@Load 1.20 kg,
Temperature 300 °C
10 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ASTM D1238
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 99.0 MPa14400 psi5 mm/min; ASTM D638
 99.0 MPa14400 psi5 mm/min; ISO 527
Elongation at Break 2.9 %2.9 %5 mm/min; ASTM D638
 2.9 %2.9 %5 mm/min; ISO 527
Tensile Modulus 5.96 GPa864 ksi1 mm/min; ISO 527
 6.10 GPa885 ksi5 mm/min; ASTM D638
Flexural Strength 147 MPa21300 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.38 GPa780 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 160 J118 ft-lbASTM D256
Izod Impact, Unnotched 6.27 J/cm11.7 ft-lb/inASTM D4812
Charpy Impact Unnotched 4.80 J/cm²22.8 ft-lb/in²ISO 179/2C
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²ISO 179/2C
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
@Thickness 3.20 mm
266 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 3.20 mm
259 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 HB
@Thickness 0.500 mm
HB
@Thickness 0.0197 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 285 - 305 °C545 - 581 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 285 - 310 °C545 - 590 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 °C230 °FInjection Molding
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hourInjection Molding
Back Pressure 0.100 - 0.300 MPa14.5 - 43.5 psi
Screw Speed 50 - 90 rpm50 - 90 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81996 / 289943

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.