MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 82 Polyethylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Bapolene® 82 is a copolymer resin with superior optical properties. This product complies with US FDA 21CFR 177.1630.

Applications: Blow Molding Applications; Bottles; Containers; Food Containers; Household Goods.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Copolymer; Good Optical Properties
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccPycnometer
Viscosity Measurement 0.72 - 0.76+/-0.02 Internal Measurement
Crystallinity >= 50 %Pycnometer
 
Chemical PropertiesOriginal ValueComments
Acetaldehyde <= 1.00 ppmGC
Diethylene Glycol <= 2.3 %GC
 
Thermal PropertiesOriginal ValueComments
Melting Point 248 °CInternal Measurement
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %Titration
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
processBlow Molding
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Dow LIGHTER™ S93 Polyethylene Terephthalate (PET) Resin
DAK Americas Laser+® C91A PET
Bamberger Polymers Bapolene® 80 Polyethylene Terephthalate
Goodfellow CVD Graphene Film on PET

PBP1111 / 81836

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.