MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals Novapol® LF-0718-A-INJECTION LDPE Injection Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: LF-0718-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. LF-0718-A is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking. This resin is biologically and chemically inert.

Features: Excellent balance of toughness and softness, Good processability and dimensional stability

Applications: Caps and closures, including tamper evident closures

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D 792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353ASTM D 2240
Tensile Strength at Break 11.0 MPa1600 psiASTM D 638
Tensile Strength, Yield 9.00 MPa1310 psiASTM D 638
Elongation at Break 548 %548 %ASTM D 638
Flexural Modulus 0.211 GPa
@Strain 2 %
30.6 ksi
@Strain 2 %
Secant; ASTM D 790
Flexural Modulus, 1% Secant 236 MPa34200 psiASTM D 790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 83.0 °C181 °FASTM D 1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips 4538B LDPE Injection Molding Resin
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips KN 230B LDPE Injection Molding Resin
NOVA Chemicals Novapol® LM-2522-A LDPE Injection Molding Resin
Chevron Phillips KN 230 LDPE Injection Molding Resin

PNOV813 / 108873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.