MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Saffil® Alumina/Silica SiO2 4/Al2O3 96
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Saffil® is produced as a fiber and was developed for thermal insulation at higher temperatures. Saffil® fiber products such as the Non-Woven Fabric and Sheet are widely used for lining high temperature furnaces, with good performance up to 1600C. Saffil® fibers show very little volume change at this temperature, as well as showing good strength and flexibility. Saffil® products are low weight materials, highly resistant to thermal shock and can rapidly reach high temperatures. They are suitable for high vacuum conditions and are resistant to acids and steam. Non-woven fabrics are similar to papers, being flexible and resilient with smooth surfaces. Typical applications include catalyst support, filtration and furnace or mold lining. Sheets (often called Tiles) are light, open rather fragile items produced by vacuum pressing, often used as preforms for impregnation to make composites. The fiber orientation is random planar parallel to the flat faces. A wider range of volume fractions can be supplied to special order.

The technical data provided is for the Saffil® fibers that make up the Sheet and Non-Woven Fabric.

Information provided by Goodfellow.

Key Words: SiO2, Al2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.30 - 3.50 g/cc0.119 - 0.126 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1000 MPa145000 psi
Tensile Modulus 100 - 300 GPa14500 - 43500 ksi
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°F
Melting Point 2000 °C3630 °F
Maximum Service Temperature, Air 1600 °C2910 °FContinuous Use
 
Component Elements PropertiesMetricEnglishComments
Al2O3 96 %96 %
SiO2 4.0 %4.0 %
 
Descriptive Properties
Chemical Resistance - AlkalisGood
Chemical Resistance - Concentrated AcidsGood
Chemical Resistance - Dilute AcidsGood
Chemical Resistance - HalogensGood
Chemical Resistance - MetalsGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Alumina Silicate SiO2 53/Al2O3 47
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2
CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Goodfellow Alumina/Silica SiO2 20/Al2O3 80
ICE Mullite, 3Al2O3-SiO2

CGOODF103 / 935

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.