General Notes on Meldin 2000 Series Bearing Products: For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin® 2000 Series can be machined into various configurations, from rod or sheet stock shapes. Black in color. Meldin® 2000 Series offers very high compression strength, high creep resistance, and dimensional stability. Specific Notes on Meldin® 2001 Bearing Meldin® 2001 is best suited for thermal and electrical insulation and radiation resistance. Meldin® 2001 has the highest compressive strength properties of any material in the series.
Applications include: Appliances, Automotive, Industrial, Semiconductor, Transportation.
Specification Notes: Note that the specifications given for this product are typical specifications for the Meldin® 2000 Series, and individual products will vary as indicated in the material notes. Information provided by Saint Gobain Performance Products. |