MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Latrobe Graph-Air® Cold Work Tool Steel (ASTM A10)
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel; Cold Work Steel

Material Notes: Graph-Air tool steel is an air-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles which impart excellent machinability and non-seizing characteristics. The graphite particles make the steel self-lubricating in dry environments, and help to retain oil in lubricated environments. Graph-Air tool steel can be hardened to over 60 Rockwell C from a relatively low hardening temperature, which minimizes size change and distortion during heat treatment. Typical applications include thread gauges, master gages, cams, bushings, sleeves, meat granulator plates, arbors, forming rolls, shear blades, punches, dies, bar feed guides and other machine tool parts.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.68 g/cc7.68 g/cc
Density 7.67 g/cc0.277 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 61615 in thickness; Air Cooled from 816°C, 120 minutes
 62623 in thickness; Air Cooled from 802°C, 60 minutes
 63632 in thickness; Air Cooled from 788°C, 45 minutes
Modulus of Elasticity 207 GPa30000 ksi
Machinability 85 - 90 %85 - 90 %1% Carbon Steel
Izod Impact Unnotched 24.4 J18.0 ft-lbAir Cooled from 788°C; 94°C Temper Temperature
 163 J120 ft-lbAir Cooled from 788°C; 594°C Temper Temperature
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.25 µm/m-°C
@Temperature 24.0 - 204 °C
7.361 µin/in-°F
@Temperature 75.2 - 399 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.94 %0.94 %
Chromium, Cr 0.50 %0.50 %
Iron, Fe 96.56 %96.56 %
Manganese, Mn 1.2 %1.2 %
Silicon, Si 0.30 %0.30 %
Tungsten, W 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type A10 Tool Steel
AISI Type A2 Tool Steel
Bohler-Uddeholm AISI D2 Cold Work Tool Steel
Schott BG3 Band Pass Filter
SKS51M Air-Hardening Tool Steel

NTIMK105 / 19452

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.