MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Radici RADILON® S RV300K 100 NT Nylon 6, 30% Glass Fiber Reinforced, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Description: PA6 30% glass fiber reinforced injection molding grade. Heat stabilized. Natural color. Suitable for parts requiring medium stiffness, good mechanical resistance and good heat ageing properties retention.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: Heat stabilized or stable to heat, UL Listed

Industries: Automotive, Consumer Industry Goods, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Water Absorption 7.5 %
@Thickness 2.00 mm
7.5 %
@Thickness 0.0787 in
Immersion at 23°C; ISO 62
Moisture Absorption 2.00 %
@Thickness 2.00 mm
2.00 %
@Thickness 0.0787 in
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inMelt Temp/Mold Temp/Cavity Pressure: 280/90/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inMelt Temp/Mold Temp/Cavity Pressure: 280/90/60; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 175 MPa25400 psi5mm/min; ISO 527-2/1A
Elongation at Break 4.0 %4.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 9.50 GPa1380 ksi1mm/min; ISO 527-2/1A
Flexural Strength 265 MPa38400 psi2mm/min; ISO 178
Flexural Modulus 8.20 GPa1190 ksi2mm/min; ISO 178
Charpy Impact Unnotched  8.50 J/cm²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 9.80 J/cm²
@Temperature 23.0 °C
46.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohm500V; IEC 60093
Comparative Tracking Index 550 V550 VSol. A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
12.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 220 °C428 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75/2Af
Vicat Softening Point 210 °C
@Load 5.10 kg
410 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Flame Spread <= 0.000 mm/min
@Thickness 3.00 mm
<= 0.000 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI135 / 313636

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.