MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake Epolene® N-14P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Epolene N-14P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss of paper coatings, aid in pigment dispersion and mold release, and improve scuff and rub off resistance in printing inks. For these applications, six Epolene N-types, differing mainly in viscosity, are available to choose from (Epolene N-10, N-11, N-14, N-30, N-34, and N-35).
    Key Attributes:
  • Aids in pigment dispersion
  • Easy to melt blend with natural or synthetic waxes
  • Improves physical properties of paper coatings
  • Increases scuff and rub off resistance in inks
  • Low density polyethylene (PE)
    Application/Uses:
  • Automotive
  • Building and Construction
  • Hot Melt Adhesives
  • Packaging
  • Solventborne Adhesives
  • Wax Modification

Information provided by Westlake Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 - 0.950 g/cc0.910 - 0.950 g/cc
Viscosity 75 - 200 cP75 - 200 cP542-111
Brookfield Viscosity 150 cP
@Temperature 125 °C
150 cP
@Temperature 257 °F
Molecular Weight 4000 g/mol4000 g/mol
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 343 °C>= 649 °FASTM E136
Ring & Ball Softening Point 108 °C226 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 2.0<= 2.0542-130
 
Descriptive Properties
Penetration Hardness3 dmmASTM D5, Needle under 100-g load for 5s @ 25 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8912 / 133457

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.