System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
AISI 8740H Steel, oil quenched 830°C (1525°F), 595°C (1100°F) temper, 100 mm (4 in.) round
Categories:
Metal
;
Ferrous Metal
;
Alloy Steel
;
AISI 8000 Series Steel
;
Low Alloy Steel
;
Carbon Steel
;
Medium Carbon Steel
Material Notes:
Post oil quenched hardness 42 HRC surface, 37 HRC half-radius, 36 HRC center
Key Words:
B.S. Type 7, UNS H87400, ASTM A304, SAE J1268, DIN 1.6546, UNI 40 NiCrMo 2 KB
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.85
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Brinell
248
Hardness, Knoop
272
Converted from Brinell
Hardness, Rockwell B
98
Converted from Brinell
Hardness, Rockwell C
23
Converted from Brinell
Hardness, Vickers
261
Converted from Brinell
Tensile Strength, Ultimate
855
MPa
Tensile Strength, Yield
670
MPa
Elongation at Break
20.5 %
in 50 mm
Modulus of Elasticity
205
GPa
Typical for steel
Bulk Modulus
160
GPa
Typical for steel.
Poissons Ratio
0.29
Calculated
Machinability
65 %
annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus
80.0
GPa
Typical for steel
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000234
ohm-cm
Typical steel
Thermal Properties
Original Value
Comments
Specific Heat Capacity
0.475
J/g-°C
Typical steel
Thermal Conductivity
46.6
W/m-K
Typical steel
Component Elements Properties
Original Value
Comments
Carbon, C
0.37 - 0.44 %
Chromium, Cr
0.35 - 0.65 %
Iron, Fe
96.435 - 97.88 %
As remainder
Manganese, Mn
0.70 - 1.05 %
Molybdenum, Mo
0.20 - 0.30 %
Nickel, Ni
0.35 - 0.75 %
Phosphorus, P
<= 0.035 %
Silicon, Si
0.15 - 0.30 %
Sulfur, S
<= 0.040 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AISI 8740 Steel, oil quenched 830°C (1525°F), 595°C (1100°F) temper, 100 mm (4 in.) round
AISI 8740 Steel, oil quenched 830°C (1525°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 8740 Steel, oil quenched 830°C (1525°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 8740 Steel, oil quenched 830°C (1525°F), 595°C (1100°F) temper, 50 mm (2 in.) round
AISI 8740H Steel, normalized 870°C (1600°F), 100 mm (4 in.) round
M874BO / 8607
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.