MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

MOL Group TIPPLEN R 1059 A Random copolymer for injection
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description: TIPPLEN R 1059 A is a random copolymer polypropylene with high flow properties for injection molding applications for high speed injection molding machines. The product shows excellent transparency and gloss. The grade contains clarifying and antistatic agent and made with special optical additive.

Applications: TIPPLEN R 1059 A is recommended for injection molding for the production of household articles, containers and thin walled packaging for cosmetics, toiletries, herbs, confectionery, where the higher gas permeability is no problem. It is applicable for injection molding of transparent food containers, which can be used in microwave oven.

(1) Average mechanical property values of several measurements carried out on standard injection-molded test specimens prepared in accordance with ISO 294-1. (2) Measured on specimen with 1 mm wall thickness

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 84 g/10 min
@Load 2.16 kg,
Temperature 230 °C
84 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 80801; ISO 2039-2
Tensile Strength, Yield 29.0 MPa4210 psi1; ISO 527-1,2
Elongation at Yield 13.5 %13.5 %1; ISO 527-1,2
Modulus of Elasticity 1.15 GPa167 ksi1, in Tension; ISO 527-1,2
Flexural Modulus 1.10 GPa160 ksi1; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²1; ISO 180/A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C192 °F1, flatwise; ISO 75-1,2
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %2; ISO 14 782
 
Processing PropertiesMetricEnglishComments
Processing Temperature 185 - 230 °C365 - 446 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG114 / 297280

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.