CAS Number: 68441 - 17 - 8 VISCOWAX® 261 – high quality oxidised, polar polyethylene wax. Application: - Plastic processing
- Paraffin compounding, candle industry
- Increase on solidification and drop points
Applications as water-based Emulsions:- Textile Industry
- Plasticizer component
- Improvement of cross-linking properties, tear resistance and smoothing of fabrics
- Slip agent for sewing threads
- Leather processing
- Additive for synthetic resin dispersion used for finishing, fulling and smoothing of upper leather
- Water-based varnishes
- Floor, shoe, furniture polishes
Information provided by Innospec Inc |